This high-temperature oil well cement retarder additive is synthesized via copolymerization of sulfonated compounds and organic acids, resulting in a product that performs reliably in a broad temperature range from 60°C to 180°C (BHCT). The recommended dosage is between 0.1% to 1.0% by weight of cement (BWOC), effectively extending thickening time and pumpability for safe placement in high-temperature environments.
Send Inquiry
Description

Product Description: High-Temperature Oil Well Cement Retarder Additive

This product is a high-performance oil well cement retarder additive specifically engineered for challenging medium to deep well cementing operations. It is a highly hydrophilic polymer that rapidly dissolves in water, ensuring quick and uniform dispersion in cement slurries. Its molecular structure features strategically designed bicarboxylic acid groups and sulfonate groups, which interact with cement phases-primarily tricalcium aluminate (C₃A) and tricalcium silicate (C₃S)-through multiple mechanisms including adsorption, chelation, dispersion, and wetting.

During the initial hydration stage, this oil well cement retarder additive preferentially adsorbs onto C₃A surfaces, effectively inhibiting its rapid reaction and thereby delaying the setting process. Simultaneously, it promotes the formation of a stable solvation film around cement particles and calcium ions through the development of an electric double layer, enhancing particle dispersion and fluidity. The sulfonate groups provide robust thermal stability, while the weak adsorption on C₃S ensures that the long-term hydration and strength development of cement are not compromised.

 

A key application of this oil well cement retarder additive is in the design of right-angle set cement slurries, which remain pumpable for an extended period before rapidly developing strength, reducing waiting-on-cement time and improving operational efficiency. It is compatible with various cement classes and other additives, making it a versatile solution for high-pressure high-temperature (HPHT) well sections.

The product should be stored in a cool, dry environment to maintain stability and performance, with a recommended shelf life of two years.

 
Specification
Appearance
No hardening particles
Moisture,%
≤8.0
Fine degree (mesh0.315mm),%
<15
G grade cement, high sulfur resistance): 800g, distilled water: 352g,ME-9S:3.2g,G301:8g, G401:12g
Thicking time ﹙90℃/53.3 MPa/49min﹚,min
≥120
Initial consistency﹙90℃/53.3 MPa/49min﹚,Bc
≤30
Thickened linear mutation value,Bc
≤10
Thickening time extension value,min
≥60
Dosage susceplibility,%
≤25
Temperature susceplibility ,%
≤20
Item
Appearance
Moisture,%
Fine degree (mesh0.315mm),%
G grade cement, high sulfur resistance): 800g, distilled water: 352g,ME-9S:3.2g,G301:8g, G401:12g
Transition time ﹙90℃/53.3 MPa/49min﹚,min
≤40
Free fluid ﹙90℃﹚,%
≤1.4

 

Hot Tags: Oil Well Cement Retarder Additive, suppliers, manufacturers, datasheet, China, USA, India, Russia, Kuwait, Saudi Arabia, cement slurry additives, slurry strength development time for cementing, cementing slurry single component additives, cementing slurry compatibility additives, cementing chemicals, slurry chemical resistance testing for cementing