The main challenges our clients always face in Toughest Drilling & MECOs Engineering and Specialty Chemicals Solutions

Every difficult well starts with a fluid decision - and that decision is made in a laboratory, not in a catalogue. At MECO the people who design the formulation are the people who make it, test it and re-test it before it ships. When the well gives you trouble, you are talking to the engineer who owns the product line.

 

page-600-340
page-600-340
page-600-340
page-600-340

Challenges from wells & Solutions from MECO

 

1-Bit balling

What the client faced

The bit stops cutting and starts chewing. Mud cakes on the bit and the BHA, the rate of penetration falls away, and the string starts to turn hard on the way up.The mechanism: Reactive clays - smectite and illite-smectite - hydrate in the water-based mud and swell. The swollen gumbo smears onto the bit faces, loads the cutting structure, and has to be broken off before the well can go further

MECO's Solution

HIB-DRIL water-based inhibitive system built around POLYAMINE DRIL liquid polyamine shale inhibitor (≤160 °C), which inhibits hydration of shale and gumbo clays and minimises bit balling, with ME NANO-LATEX nano-latex sealant (≤160 °C) sealing micro-fractures and pores. For soft, sticky gumbo, HEM-DRIL with EP LUB HEM metal-wetting lubricant (≤180 °C).

Where to go finding out data?→ /shale-inhibitors/ · /lubricants

Case study Yang 102 H36-2 block(Sichuan gas field):reduced 24 days than the plan and 4 days shorter than the first super dual-row horizontal well

 

2-Torque & drag (T&D) and stuck pipe

What the client faced:

Torque climbs past the rig limit on the way in, drag climbs on the way out, the build section stalls, and in a long lateral the pipe can stop halfway.

Each stuck-pipe event costs days.The mechanism: In the build section and the lateral the drillstring lies against the low side of the wellbore over thousands of metres.

Friction accumulates where lubricity is low, the filter cake is thick and soft, and cuttings beds load the hole.

MECO's Solutions

FORCLE DRIL formate-based reservoir drill-in fluid with ROP DRIL ROP enhancer (≤180 °C) that reduces bit and BHA balling and lowers torque and drag. HEM-DRIL adds EP LUB HEM lubricant (≤180 °C) for soft, sticky gumbo shales. HIB-DRIL adds SOLTEX DRIL HIB sulfonated asphalt shale inhibitor (≤180 °C): low friction coefficient for laterals, thin filter cake.

Where to go finding out data?→ /forcle-dril/ · /lubricants/

Case study" H90-3(CNPC Changqing Oilfield):Touque & Drag reducted around 50% than the neighbour well,frictional resistance dropped 80%,finished the drill in horizontal well 2,269 m smoothly.

 

3-Cuttings suspension and solid control

What the client faced:

Cuttings bed on the high side of the horizontal, come back in pulses, and raise the effective density of the fluid column. Shaker screens overload, dilution rates climb, and the pressure surface goes erratic.The mechanism: In deviated and horizontal sections gravity-driven

settling creates cuttings beds that periodically avalanche.

Each avalanche produces a pressure surge, an ECD excursion, and a step change in torque and drag

MECO's Solutions

SUPER DRIL formate-based clay-free low-ECD polymer and sulfonate fluid with LIQUIT FLC (≤190 °C) dual-function high-temperature polymer for viscosity and filtration control, and XC POLYMER HT (≤160 °C) modified xanthan with higher LSRV under high temperature for annular suspension in long horizontal intervals. HEM-DRIL with VIS LSRV (≤190 °C) branched synthetic polymer viscosifier extends conventional systems beyond normal temperature limits

.Where to go finding out data?→ /viscosifiers-suspension-agents/ · /showroom/synthetic-based-drilling-fluids-additives/Case study West II H4-1(SINOPEC):180 °C Borehole no sag,Tunnel viscosity 40–50 s,6,941 m / 2.34 g/cm³,Increased ROP 10%.

 

4 -Equivalent circulating density

(ECD) and the pressure window

What the client faced

The margin between the ECD and the fracture gradient shrinks until a single pump-rate change is enough to fracture the formation - or to lift the well underbalanced.

Either way the operation stops.The mechanism: Annular pressure loss from fluid rheology and cuttings loading pushes the effective circulating density up.

In a long lateral the window is narrow, and the fluid that behaves at surface is not the fluid that behaves at bottomhole temperature.

MECO's Solutions

FLAT ECD DRIL with RHE-O-MOD rheology modifier (≤180 °C) maintains consistent plastic viscosity and yield point across the temperature range, and THIN DRIL sulfonate thinner (≤190 °C) conditions flat-rheology systems. For invert-emulsion service, CLAY VIS PLUS organo-amine bentonite (200 °C) holds viscosity and suspension, and LIGNITE RXDRIL organophilic lignite (220 °C) reduces HPHT filtration in invert systems.

Where to go finding out data?→ /specialty-chemicals/rop-rapido-rop-enhancer.html · /thinners-and-dispersants/

 

5-Lost circulation

What the client faced

Fluid reclamation drop, the pit level falls, and the pump pressure falls with it. The loss may be in a fractured interval, a vuggy one, or a depleted one - and the next pump rate may open it wider.

The mechanism: Losses occured by different mechanisms: induced fractures from excessive ECD, pre-existing natural fractures, and vugs or thief zones. One bridging material does not fit all three.

The material has to match the loss mechanism and the width of the opening.

MECO's Solution

MECO's lost-circulation materials work on the mechanism - bridge plugging, then stress equalisation - ME-NEP is an wellbore strengthening material engineered to effectively seal micro-fractures and permeable formations

On the fluid side the pressure that opens the loss is held down by SUPER DRIL clay-free low-ECD formate system and FLAT ECD DRIL with RHE-O-MOD (≤180 °C); ME NANO-LATEX (≤160 °C) seals micro-fractures and pores as they open.

Where to go finding out data?→ /lost-circulation-materials/ Filtration control agent· /showroom/

swellable-hydratable-lcm-s-combinations-in-kuwait/

 

6-Formation influx (well kick)

What the client faced

The problem of casing :The pit volume rises and the flow shows gas. Foam comes back with it, the mud weight was not designed for the influx, and in a sour well the downhole casing shows pitting corrosion by acid gas (H₂S/CO₂) exposure.

The problem of influx : An influx starts when static bottomhole pressure falls below pore pressure - the well heats up, the mud is diluted, or the formation is over-pressured. Then gas migrates up and breaks out as foam, while acid gas dissolves in, consuming alkalinity and corroding casing.

H2S STOP

MECO's Solution

RHE-O-MOD (≤180 °C) in FLAT ECD DRIL holds plastic viscosity and yield point across temperature, so ECD does not drift.

DEFOA GAS keeps migrating gas from breaking out as foam.

H2S STOP (triazine base) scavenges provides an effective neutralization of H₂S ;

FILMING AMINE, ≤204 °C monovalent / ≤149 °C divalent brine) protects steel of casing from CO₂ and H₂S.

Find out Specialty chemicals

ECD reduction for extended-reach wells → /specialty-chemicals/rop-rapido-rop-enhancer.html DEFOA-GAS → /defoamers-surfactants/non-alcohol-organic-silica-based-defoamer.html

Filming Amine & H2S STOP (Sour-gas treatment) → /Specialty chemicals list /FILMING AMINE/-H2S STOP-triazine-based-high-performance.html

 

7-Return permeability

What the client faced

The well is completed and the production rate is below what the reservoir should give.

The skin effect is there, and it is chemical rather than mechanical.The mechanism:

The filter cake that held pressure against the formation during drilling becomes the barrier to production. Where it is thick, permeable, or incompatible with the completion fluid, the near-wellbore permeability does not come back.

MECO's Solution

FORCLE DRIL formate-based reservoir drill-in fluid built for low permeability, with SUPER DRIL and POLY HT (≤190 °C) composite divalent-salt fluid combining shale stability, return permeability and reduced corrosion.

OBM CLEAN PACKAGE, WBM CLEAN PACKAGE & CAKE-Caco3-breaker is designed for clean up the filter cake compatible with different formation, facilitating maximum efficiency of the Filter Cake Breaker Treatment.

Where to go finding out data?→ /drill-in-solutions · /specialty-chemicals/prd-system-protecting-reservoir-drill-in.html

 

8-High-temperature rheology control

What the client faced

The fluid viscosity collapse in downhole, the suspension fails, and cuttings drop out before they reach the shaker. The cake degrades, fluid loss rises, and the mud report no longer matches the design.

The mechanism: Above 160–180 °C most water-based polymers is thermal degraded, chain scission and gel. The fluid stops working before the well does.

MECO's Solution

VeraTherm Fluid with VIS LSRV HT (≤190 °C) viscosifier and RESINATED LIGNITE (≤190 °C) lignite-resin filtrate reducer and stabiliser. In invert systems, CLAY VIS PLUS holds viscosity and suspension to 200 °C for 100 hours with flat thermal stability, and LIGNITE RXDRIL controls HPHT filtration to 220 °C. LIGNO LS (≤190 °C) lignosulfonate deflocculant acts as gel-strength reducer and stabiliser.

XC POLYMER HT Provides superior LSRV in saltwater at high temp.

Where to go finding out data?→ /thermally-stable-specialties · /viscosifiers-suspension-agents/Case study: Hua 3 Gas field(Sichuan):BHT 202.5 °C,116 MPa,6,540 m,Veratherm Fluid saved the owners cost around 2/3 of current.

 

9-HTHP Filtrate Loss in DF & RDF

What the client faced

In HTHP well sections, mud loses water to the formation under the influence of a pressure differential; solid particles remain attached to the wellbore wall and accumulate layer by layer, forming a filter cake. The overlying rock formation requires a filter cake with low water loss and a thin, tough structure: the thickness of the filter cake directly determines differential adhesion (≈ filter cake thickness × pressure differential × frictional difference); excessive thickness causes pressure-differential stucking, while insufficient pressure differential can lead to wellbore wall collapse and an increase in wellbore diameter.

MECO's Solution

VeraTherm SYSTEM with RESINATED LIGNITE (≤190 °C) filtrate reducer and VIS LSRV HT (≤190 °C) for a thin, ultralow-permeability cake;

SUPER DRIL with LIQUIT FLC (≤190 °C) in clay-free formate drill-in; FLAT ECD DRIL with LIQUIT TROL HT (≤170 °C) and LIGNITE RXDRIL (220 °C) for HPHT loss in invert.

VESA THERM DRIL with LIGNITE RXDRIL

Where to go finding out data?→

Filtrate reducers matched to the temperature window → /filtration-control-agents/

The clay-free PRD system for reservoir drill-in → /specialty-chemicals/prd-system-protecting-reservoir-drill-in.html /How MECO builds a reservoir drill-in fluid → /drill-in-solutions/

 

 

10-Filter cake removal

What the client faced

The reservoir section requires a permeable, recoverable, or acid-soluble cake-tight, low-permeability cake , enabling direct pressure production capacity.

The well is flowed back and the filter cake does not dissolve. Production comes in below expectation, and the cause is the very layer that protected the formation while it was drilled.

The mechanism: A cake that is stable against the drilling fluid can still be stable against the completion brine or the acid stage.

The damage then carries from the drilling operation straight into the production interval.

MECO's Solution

MECO's cake-breaker range :OBM CLEAN , WBM CLEAN &OILWET-BREAK is designed for clean up the filter cake compatible with different formation, facilitating maximum efficiency of the Filter Cake Breaker Treatment.

On the fluid side, HIB-DRIL with SOLTEX DRIL HIB (≤180 °C) gives a thin filter cake, and the VeraTherm system's VIS LSRV HT (≤190 °C) an ultralow-permeability one.

Where to go finding out data?→ /specialty-chemicals/filter-cake-breaker-removal.html · /specialty-chemicals/obm-filter-cake-breaker.html · /specialty-chemicals/obm-filter-cake-caco3-breaker.html

 

Specialty Chemicals list

 

Each pairing below is based on the published specifications of the third-party product as of date between 2022-2026 and MECO's own test data for the stated test method. Individual results vary with mud system, temperature and treatment. This table does not imply affiliation, endorsement, authorisation, or a drop-in replacement of any third-party product. Supporting test data are available on request

 

No.

Product name & Code

Code of MECO System

Profile of performance in the System

1

Thermal stable xanthan gum(XC POLYMER HT)

HIB-DRIL & Format base Drill-in Fluid/ Comparable to DUO-VIS

Unconventional wells ,deviated and horizontal wells, reactive shale plays. Provides superior LSRV in saltwater, including KCl, field brines, seawater, and workover and completion fluids Thermal stable up to 160°C with thermal extender

2

Water-based drilling fluid with high-temperature shale inhibitor resistance( POLYAMINE DRIL )

HIB-DRIL & HEM-DRIL/Comparable to KLA-STOP

liquid polyamine shale additive is used in polymer-based drilling and drill-in fluids,effectively inhibits shale or gumbo clays from hydrating and minimizes the potential for bit balling. while drilling and running pipe, Thermal stable up to 160°C

3

Modified Starch as filtration loss agent. STARCH DRIL

HEM-DRIL & LOSH-DRIL / Comparable to AKVOTROL

It is designed as a fluid loss control additive in drilling fluids where biocides are not permitted but resistance against fermentation & high temperature stability are required, Thermal stable up to 160°C

4

Water-based drilling fluid encapsulating(PHPA DRIL HIB, PHPA DRIL HEM)

HIB-DRIL & HEM-DRIL /Comparable to ULTRA CAP

Provides excellent cuttings encapsulation by adsorbing onto clay surfaces and forming a protective film that prevents cuttings from sticking to each other or to the shaker screens.Thermal stable up to 160°C

5

Water-based mud rate of penetration enhencer ( ROP DRIL )

Forcle Dril/ Comparable to DRILZONE

ROP DRIL not only reduces bit and bottomhole assembly (BHA) balling, but also lowers torque and drag, It is especially applicable when drilling medium-to-hard shales in both onshore and offshore operations.Thermal stable up to 180°C

6

Shale inhibitor Agent for Water-based Drilling Fluids, Sulfonated Asphalt(SOLTEX DRIL HIB)

HIB DRIL/Comparable to ASPHASOL Supreme

Shale inhibition
Low coefficient of friction factors for laterals
Stable, low-shear viscosity
Thin, high-quality filtercake ,thermal stable up to 180°C

7

Branched synthetic polymer viscosifier (VIS LSRV )

HEM-DRIL/ Comparable to veravis

Viscosifire ,Thermal stability
·Flexibility that extends conventional systems beyond their
normal limits,thermal stable up to 190°C

8

Polymer & sulfite compound gel modifier & filtrate loss control agent(LIQUIT FLC)

SUPER DRIL/Comparable to BaraVis W-637

A dual function, high-temperature polymer that provides optimum viscosity and filtration control. use in Clay-free formate base fluid

9

Lubricant for Water-based Drilling Fluids (EP LUB HEM)

HEM DRIL / Comparable to LUBE-167

Contains unique metal-wetting additives which reduce the tendency of soft, sticky shales (gumbos) to cause bit and BHA balling,thermal stable up to 180°C

10

Water-based drilling fluid with high-temperature resistant viscosity enhancer(VIS LSRV)

VeraTherm SYSTEM /Comparable to VERAVIS

Exhibits an excellent rheological profile with elevated low-end readings ,provides fluid loss control and helps produce a thin, ultralow-permeability filtercake.thermal stable up to 190°C

11

Composite divalent salt drilling fluid: an anti-high-temperature drilling fluid with filter loss reduction properties (POLY HT)

SUPER-DRIL / Comparable to DRISTEMP D Polymer,

Shale stability
Excellent return permeability
·Reduced corrosion rates
·Lubricity,thermal stable up to 190°C. Tolerate in mono & divalent & HTHP brine

12

Filtrate Reducer for Water-based Drilling Fluids, Lignite Resin( RESINATED LIGNITE)

VeraTherm SYSTEM/Comparable to RESINEXII

Bottomhole temperature stabilizer
Controls fluid loss in basically all water-based drilling fluidsSystem,thermal stable up to 190°C

13

Sodium petroleum sulfonate type OBM Thinner (THIN DRIL )

FLAT ECD DRIL ,thermal stable up to 190°C/ Comparable to VERSATHIN HF

Used as a thinner and conditioner in the FLAT ECD DRIL ,Equal to RHELIANT SLB, flat-rheology drilling fluid system

14

Lignosulfanates type WBM Thinner (LIGNO LS)

HT-HPWBM/ Comparable to SPERSENE

A multipurpose deflocculant and gel-strength reducer, temperature stabilizer, and filtration-control additive

15

Oil-based drilling fluid filtrate loss reducer (LIGNITE RXDRIL )

VESA DRIL /FLAT ECD DRIL,thermal stable up to 190°C/ Comparable to BaraFLCIE 514

Equal to Onetrol SLB /Versadrill oil-based system

16

Liquid Nano polymer-based filtrate reduction agent for oil-based drilling fluids(LIQUIT TROL HT)

HYPER DRIL ,thermal stable up to 170°C/ Comparable to MEGADRIVE F

Reduces HPHT fluid loss at temperaturesup to 190 degC]
Exhibits superior HTHP fluid loss control
at low product concentrations

17

Organic amine-modified bentonite( CLAY VIS PLUS F),BENVIS

FLAT ECD DRIL / Comparable to VG PLUS (RHELIANT plus system

thermal stable up to 190°C

18

Integrated Emulsifier for Oil-based Drilling Fluids( EMUL DRIL PLUS ),

VESA DRIL /FLAT ECD/Comparable to SUREMUL PLUS

One drum emulsifier, ,thermal stable up to 190°C

19

Organic amine-modified bentonite(CLAY VIS PLUS V)

VESA DRIL DRILComparable to VERSAGEL

Stable rheologies in tandem with ultra-thin and slick filter cake deposits clear the path for efficient logging, casing and cementing operations.,stable up to 200°C/

20

Oil-based drilling fluid wetting agent(O-WET DRIL )

FLAT ECD DRIL/Comparable to Surewet

Wetting of solids to avoid barite sag .stable up to 160°C

21

Polymeric filtrate reducer for oil-based drilling fluids, solid(ME Nano-latex)

FLAT ECD DRIL/ Comparable to ECOTROL HT

Polymer powder with micro size as subsitute for gilsonite ,no gelation under high temp . stable up to 160°C

22

OBM Rheology modifier (RHE-O-MOD)

FLAT ECD DRIL/ Comparable to RHEFLAT PLUS

Rheology modifier stable up to 160°C

23

H2S STOP

 

Triazine base scavenges, provides an effective neutralization of H₂S ;

24

FILMING AMINE,

CONQOR 101

Amine base Corrosion inhibitor ≤204 °C monovalent / ≤149 °C divalent brine, protects steel of casing from CO₂ and H₂S.

25

OBM CLEAN ,

SAFE-SOLV

Fast-acting hydrocarbon solvent additive combines nonaromatic hydrocarbon and natural terpene solvents and surfactants for rapid grease solvency with less contact time

26

WBM CLEAN

BREAKDOWN/ D-SOLVER HD

This package of WBM CLEAN Clean up the starch additive and the calcium carbonate bridging material., clean up the filter cake in open hole.

27

OILWET-BREAK

FAZE-OUT

Convert the filtercake of an oil- or synthetic-based reservoir-drill-in fluid (RDF) from an oil-wet to a water-wet state for easier and quicker removal

Send Inquiry